MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Insulcast® MRTV 2 Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST MRTV 2 is a high tear strength, high elongation, addition cure mold-making RTV silicone rubber. MRTV 2 has very low shrinkage on cure. The MRTV 2 is ideal for detailed reproduction.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncured. Part B
 1.15 g/cc1.15 g/ccUncured. Part A
Viscosity 10000 cP10000 cPPart B; ASTM D1084
 11000 cP11000 cPPart A; ASTM D1084
 90000 cP90000 cPPart A, Part B, mixed, uncured; ASTM D1084
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040ASTM D2240
Tensile Strength 4.83 MPa700 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
Compressive Strength 0.621 MPa90.0 psi
Tear Strength 15.8 kN/m90.0 pliDie B; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.60e+15 ohm-cm1.60e+15 ohm-cmASTM D257
Dielectric Constant 2.94
@Frequency 1000 Hz
2.94
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.00020
@Frequency 1000 Hz
0.00020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 420 µm/m-°C233 µin/in-°F
Thermal Conductivity 0.311 W/m-K2.16 BTU-in/hr-ft²-°F
 0.311 W/m-K2.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 120 min
@Temperature 65.0 °C
1.00 - 2.00 hour
@Temperature 149 °F
option
 180 - 240 min
@Temperature 50.0 °C
3.00 - 4.00 hour
@Temperature 122 °F
option
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
option
Pot Life  2.00 min
@Temperature 25.0 °C
2.00 min
@Temperature 77.0 °F
Part A. 100 g
 2.00 min
@Temperature 25.0 °C
2.00 min
@Temperature 77.0 °F
Part B. 100g
Shelf Life 6.00 Month6.00 MonthPart A
 6.00 Month6.00 MonthPart B
 
Descriptive Properties
Colorclearpart B, uncured
 whitepart A, uncured
Mix Ratio by weight100:10Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9112 / 239622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.