MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® 2103-70A Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Formerly Pellethane

Feature: High MVTR

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Lubrizol acquired the Pellethane product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0050 cm/cm0.0040 - 0.0050 in/inASTM D955
Linear Mold Shrinkage, Transverse -0.00300 - 0.0080 cm/cm-0.00300 - 0.0080 in/inASTM D955
Melt Flow 11 g/10 min
@Load 8.70 kg,
Temperature 224 °C
11 g/10 min
@Load 19.2 lb,
Temperature 435 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 69 - 7569 - 75ASTM D2240
Tensile Strength, Ultimate 24.7 MPa3580 psiASTM D412
Elongation at Break 730 %730 %ASTM D412
50% Modulus 2.10 MPa
@Strain 50 %
2.10 MPa
@Strain 50 %
ASTM D412
100% Modulus 3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ASTM D412
300% Modulus 5.20 MPa
@Strain 300 %
754 psi
@Strain 300 %
ASTM D412
Tear Strength 53.0 kN/m302 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3.03.0H22 Wheel, 1000g; ASTM D1044
Compression Set  25 %
@Temperature 25.0 °C,
Time 79200 sec
25 %
@Temperature 77.0 °F,
Time 22.0 hour
ASTM D395, Method B
 75 %
@Temperature 70.0 °C,
Time 79200 sec
75 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395, Method B
Tensile Set 50 %50 %Elongation set after break; ASTM D412
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 175 µm/m-°C
@Temperature 20.0 °C
97.2 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Vicat Softening Point 75.6 °C168 °F120°C/hr, 9.8N; ASTM D1525
Glass Transition Temp, Tg -69.0 °C-92.2 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 188 - 204 °C370 - 399 °FExtrusion
 193 - 210 °C379 - 410 °FMolding
Mold Temperature 16.0 - 60.0 °C60.8 - 140 °F
Drying Temperature 82.0 - 93.0 °C180 - 199 °Fair dew point <-40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer

PDW266a / 138259

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.