MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CEN® Electronic Material CF 150CF019 Polyimide Film
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, and enhances chemical resistance.

Applications: require a heat bondable film, or moisture and chemical resistance beyond the capabilities of uncoated CEN®CN films, such as tubing, heater circuits, heat sealable bags, automotive diaphragms and manifolds, magnetic wire, PTC Insulation

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 22.0 - 28.0 microns0.866 - 1.10 milBase; ASTM D374
 34.5 - 40.5 microns1.36 - 1.59 milTotal; ASTM D374
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 160 MPa>= 23200 psiASTM D882
Elongation at Yield >= 45 %>= 45 %ASTM D882
Peel Strength >= 0.240 kN/m>= 1.37 pliIPC-TM-650
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Strength >= 200 kV/mm>= 5080 kV/inASTM D149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Caplinq LINQTAPE™ PIT2A
Caplinq LINQTAPE™ PIT1S
Caplinq LINQTAPE™ PIT1A
Caplinq LINQTAPE™ PIT2S
CEN® Electronic Material BL Polyimide Film

PCENE007 / 93469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.