MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1070 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; High Carbon Steel

Material Notes: Applications include springs for upholstered furniture and automotive seats and backs.

Key Words: UNS G10700, AMS 5115, ASTM A29, ASTM A510, ASTM A576, ASTM A682, MIL SPEC MIL-S-11713 (2), SAE J403, SAE J412, SAE J414, DIN 1.1231, AFNOR XC 68 (Fr), SS14 1770 (Sweden), SS14 1778 (Sweden)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 212212
Hardness, Knoop 235235Converted from Brinell
Hardness, Rockwell B 9494Converted from Brinell
Hardness, Rockwell C 1616Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 223223Converted from Brinell
Tensile Strength, Ultimate 703 MPa102000 psi
Tensile Strength, Yield 385 MPa55800 psi
Elongation at Break 12 %12 %in 50 mm
Reduction of Area 30 %30 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000168 ohm-cm
@Temperature 0.000 °C
0.0000168 ohm-cm
@Temperature 32.0 °F
condition of specimen unknown
 0.0000230 ohm-cm
@Temperature 100 °C
0.0000230 ohm-cm
@Temperature 212 °F
condition of specimen unknown
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.6 µm/m-°C
@Temperature 0.000 - 100 °C
6.44 µin/in-°F
@Temperature 32.0 - 212 °F
 12.6 µm/m-°C
@Temperature 0.000 - 200 °C
7.00 µin/in-°F
@Temperature 32.0 - 392 °F
 13.3 µm/m-°C
@Temperature 0.000 - 300 °C
7.39 µin/in-°F
@Temperature 32.0 - 572 °F
 14.0 µm/m-°C
@Temperature 0.000 - 400 °C
7.78 µin/in-°F
@Temperature 32.0 - 752 °F
Specific Heat Capacity 0.490 J/g-°C
@Temperature >=100 °C
0.117 BTU/lb-°F
@Temperature >=212 °F
condition unknown
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.65 - 0.75 %0.65 - 0.75 %
Iron, Fe 98.26 - 98.75 %98.26 - 98.75 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1070 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1060 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1050 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1030 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round

M1070B / 7074

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.