MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Hyflon® MFA D5220X Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Hyflon D5220X is a white aqueous MFA dispersion. It is designed for impregnation processes and is particularly recommended for production of fabrics and laminates. Hyflon D5220X exhibits excellent wetting properties and high shear stability. Hyflon D5220X has very good film forming behaviour and is especially suited for top-coat passes to produce final items with superior gloss. Due to its features, D5220X can of course also find use in formulations for coating applications. Main features of Hyflon D5220X MFA dispersion are: - Very low APFO content - NO polyethoxylated alkylphenols - Excellent wetting properties - Superior gloss of final items

Additional Information: Processing - Hyflon D5220X is processed according to methods generally used for conventional impregnation technology. Generally the procedure involves dip-coating and then heating to remove water and surfactant from the impregnated item. Depending on the application, sintering above the melting point of the coated resin may be carried out to obtain the finished coated articles. - Hyflon D5220X can be processed neat or appropriately formulated. Also, it can be used diluted using distilled or deionized water. Formulation, line speed and oven temperature must all be well controlled for optimized features of the coated substrates. Storage and Handling - Hyflon MFA dispersions must be stored under suitable temperature conditions to ensure prolonged stability. Temperatures lower than 5°C must be avoided to prevent irreversible settling. Also, some settling may occur on prolonged standing and/or heat exposure. It is therefore strongly recommended that the product is always kept at temperatures below 35°C. The optimum storage temperature range is 10 - 25°C. It is also advisable that the product is homogenized by gentle rolling or stirring once per month and prior to use. - Prolonged exposure of the liquid to air could lead to some coagulation at the surface due to water evaporation. For this reason and also to avoid contamination, it is recommended to keep the containers closed when not in use. Safety and Toxicology - Before using Hyflon MFA dispersions consult the product Material Safety Data Sheet and follow all label directions and handling precautions. - As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Venting units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapour or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging - Hyflon D5220X is packaged in either 25 kg drums or 1500 kg IBC's.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ASTM D4441
Particle Size 180 µm180 µmAverage; Internal Method
pH >= 9.0>= 9.0ASTM D4441
Brookfield Viscosity 20 cP20 cP20°C; ASTM D2196
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FASTM D4591
 
Descriptive Properties
APFO Content< 50 ppm
AppearanceWhite
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
FeaturesHigh Gloss
 Rapid Wetting
FormsLiquid
GenericPerfluoropolymer
MFA Content55.0 wt%on the mixture; ASTM D4441
Non Ionic Surfactant3.5 wt%on the mixture; ASTM D4441
UsesCoating Applications
 Fabrics
 Laminates

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Hyflon® F1540 Perfluoropolymer
Beijing Evergrow Resources PTFE Tube and Pipe
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
Chemours Viton® F-605C Fluoroelastomer (FKM)
Chemours Viton® F-601C Fluoroelastomer (FKM)

PSOL8Y7664 / 135727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.