System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Chevron Phillips Marlex® M151 LLDPE Pipe and Corrugated Extrusion Resin
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
Linear Low Density (LLDPE)
;
Linear Low Density Polyethylene (LLDPE), Extrusion Grade
Material Notes:
Characteristics:
Good long-term hoop strength
Extended outdoor life
Clean N550 carbon black
Applications:
Pipes
Not recommended for contact with food products
Information provided by Chevron Phillips.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.918
g/cc
0.0332
lb/in³
Base Density; ASTM D1505
Carbon Black Loading
35 %
35 %
ASTM D1603
Melt Flow
12
g/10 min
12
g/10 min
Condition 190/2.16, HLMI; ASTM D1238
Melt Index of Compound
2.0
g/10 min
2.0
g/10 min
Condition 190/2.16; ASTM D1238
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin
Avient PolyOne® 2107 Black PEC Black Polyethylene
Chevron Phillips Marlex® M250 Linear Low Density Polyethylene Black Concentrate
Chevron Phillips Marlex® KN 226 LDPE Injection Molding Resin
Chevron Phillips Marlex® K606 High Density Polyethylene
PCHEVD044 / 20648
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.