MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UNS C81300, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Sum of Copper and named elements should total a minimum of 99.5%.

Casting methods recommended for this alloy: Centrifugal, Continuous, Investment, Permanent Mold, Plaster, and Sand.

Applications: Higher hardness electrical and thermal conductors.

Mechanical properties typical for separately cast heat-treated (TF00 temper) test bars.

Inactive per the Copper Development Association.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.81 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 8989500 kg, typical
Tensile Strength, Ultimate >= 365 MPa>= 52900 psi
Tensile Strength, Yield >= 250 MPa
@Strain 0.2 %
>= 36300 psi
@Strain 0.2 %
Elongation at Break >= 11 %>= 11 %in 50 mm
Modulus of Elasticity 110 GPa16000 ksi
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000002874 ohm-cm
@Temperature 20.0 °C
0.000002874 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.390 J/g-°C0.0932 BTU/lb-°F
Thermal Conductivity 260 W/m-K
@Temperature 20.0 °C
1800 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1066 - 1093 °C1951 - 1999 °F
Solidus 1066 °C1951 °F
Liquidus 1093 °C1999 °F
Shrinkage 2.1 %2.1 %Patternmaker's Shrinkage (1/4 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 260 °C500 °FStress-Relieving Temperature
Solution Temperature 980 - 1100 °C1800 - 2010 °FHeat-treating
Aging Temperature 480 °C896 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.020 - 0.10 %0.020 - 0.10 %
Cobalt, Co 0.60 - 1.0 %0.60 - 1.0 %
Copper, Cu >= 98.5 %>= 98.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
UNS C80100, Copper Casting Alloy
UNS C81100, Copper Casting Alloy
UNS C80900, Copper Casting Alloy
UNS C80300, Copper Casting Alloy
UNS C80700, Copper Casting Alloy

MC81300b1 / 11857

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.