MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont™ Nomex® 455 (NOMEX III) Aramid Staple Fiber
Categories: Other Engineering Material; Composite Fibers; Polymer; Thermoset; Aramid

Material Notes: Type 455 staple of NOMEX, a patented blend of NOMEX and KEVLAR brand fibers, was introduced to fill the need for higher performance thermal protective apparel. Type 450 staple. However, because of its lower crystalinity, it produces yarn and fabrics that are slightly lower in strength than those produced from Type 450 staple. Advantages versus Type 450 include:
  • Increased resistance to break open under thermal load. The presence of 5% KEVLAR inhibits thermal shrinkage, thus reducing the probability of break-open and the subsequent loss of the protective barrier.
  • Easier dyeability. Type 455 NOMEX can be uniformly dyed in fabric or yarn form to the many colors required for civilian protective apparel. Type 455 NOMEX is sold as a dye merged staple.
  • Fabric Appearance. Crease retention and wrinkle resistance can be imparted to NOMEX III or NOMEX IIIA by autoclaving pressed garments at 30 psig steam pressure. Although not as strong as the provide significant advantages in appearance and ease unautoclaved garments.

General NOMEX Information: Nomex® is a family of aromatic polyamide (aramid) fibers. This family consists of staple fibers, continuous filament yarns, paper, and spunlaced fabrics. Uses for staple, yarn, and spunlaced fabrics include apparel fabrics to protect against flash fire and electric arcs exposure; firefighter garments; fabrics and spun yarns for filtration applications; insulation in fire resistant thermal protective apparel; rubber reinforcement; and in transportation textiles such as airline carpeting. Some uses for paper product include insulation in electric motors and transformers, wire wrapping, and honeycombed strength members in many aircraft. Nomex® brand fibers are inherently flame resistant: the flame resistance is a polymer property and does not diminish with the life of the fiber. The fiber's low stiffness and high elongation give it textile-like characteristics which allow processing on conventional textile equipment.

Nomex® meta-aramid, poly(meta-phenyleneisophthalamide), is prepared from meta-phenylenediamine and isophthaloyl chloride in an amide solvent. It is a long chain polyamide in which at least 85% of the amide linkages are attached directly to two aromatic rings. The meta oriented phenylene forms bends in the polymer chain, reducing chain rigidity as compared to the para orientation in the chemically similar Kevlar® chain. This flexible polymer chain gives Nomex® more textile-like qualities while retaining high temperature properties similar to Kevlar®.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption at Equilibrium 4.5 %4.5 %Billed (Commercial, ASTM)
 8.3 %8.3 %fiber as shipped
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 310 MPa45000 psiCalculated from tenacity
Elongation at Break 21 %21 %Filament yarn tested at 3 TPI, 10" gauge length and 60%/minute extension rate. DuPont Test Method 12002.
Tenacity 0.229 N/tex2.60 g/denierStraight test - filament yarn tested at 3 TPI, 10 inch gauge length and 60%/min extension rate. DuPont Test Method 12002
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
10.0 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.09 J/g-°C0.261 BTU/lb-°FModulated DSC, ASTM TM E1269.
Shrinkage 0.50 %
@Temperature 100 °C
0.50 %
@Temperature 212 °F
in water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Nomex® 450 Aramid Staple Fiber
DuPont™ Nomex® 430 1200 Denier Aramid Yarn
DuPont™ Nomex® 462 (NOMEX IIIA) Aramid Staple Fiber
DuPont™ Nomex® N301 Nomex® Aramid Staple Fiber
DuPont™ Kevlar® 49 Aramid Fiber

PDUNOM3 / 33421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.