MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kumho-Sunny HSP8620G PS/PPE, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: HSP8620G is 20% GF reinforced PS/PPE resin. HSP8620G has high heat resistance, high rigidity, excellent creep performance in low and high temperature, low water absorption and high shape resistance property. HSP8620Gis mainly used in electron & electric parts, OA appliance, fluid engineering, etc.

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Maximum Moisture Content 0.100.10
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 5.0 - 8.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
5.0 - 8.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 91.0 MPa13200 psiASTM D638
Elongation at Break 10 %10 %ASTM D638
Flexural Strength 123 MPa17800 psiASTM D790
Flexural Modulus 5.21 GPa756 ksiASTM D790
Izod Impact, Notched 1.30 J/cm
@Thickness 3.20 mm
2.44 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 113 °C235 °FASTM D648
Vicat Softening Point 145 °C293 °FB; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 260 - 270 °C500 - 518 °F
Nozzle Temperature 255 - 265 °C491 - 509 °F
Melt Temperature 250 - 290 °C482 - 554 °F
Mold Temperature 50.0 - 80.0 °C122 - 176 °F
Drying Temperature 90.0 - 110 °C194 - 230 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
Back Pressure 0.200 - 0.800 MPa29.0 - 116 psi
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKMSN162 / 281014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.