MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ EX39 ABS (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Highest impact extrusion ABS for sheet and blow molding applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccASTM D792
Viscosity 1.52e+6 cP
@Shear Rate 100 1/s,
Temperature 240 °C
1.52e+6 cP
@Shear Rate 100 1/s,
Temperature 464 °F
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
0.0070 - 0.0090 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 28.0 MPa4060 psi5 mm/min; ASTM D638
Tensile Strength, Yield 35.0 MPa5080 psi5 mm/min; ASTM D638
Elongation at Break 108 %108 %5 mm/min; ASTM D638
Elongation at Yield 3.5 %3.5 %5 mm/min; ASTM D638
Tensile Modulus 1.68 GPa244 ksi5 mm/min; ASTM D638
Flexural Yield Strength 57.0 MPa8270 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.90 GPa276 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.64 J/cm8.69 ft-lb/inASTM D256
 3.20 J/cm
@Temperature -30.0 °C
5.99 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 39.0 J28.8 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 101 µm/m-°C
@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature -40.0 - 40.0 °C
65.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
@Thickness 3.20 mm
196 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 3.20 mm
171 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 106 °C223 °FRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °C140 °FUL 746B
UL RTI, Mechanical with Impact 60.0 °C140 °FUL 746B
UL RTI, Mechanical without Impact 60.0 °C140 °FUL 746B
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0598 in
UL 94
 
Processing PropertiesMetricEnglishComments
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 195 - 210 °C383 - 410 °FSheet Extrusion
 190 - 220 °C374 - 428 °FExtrusion Blow Molding
Zone 2 190 - 220 °C374 - 428 °FExtrusion Blow Molding
 200 - 220 °C392 - 428 °FSheet Extrusion
Zone 3 190 - 220 °C374 - 428 °FExtrusion Blow Molding
 205 - 230 °C401 - 446 °FSheet Extrusion
Zone 4 190 - 220 °C374 - 428 °FExtrusion Blow Molding
 210 - 235 °C410 - 455 °FSheet Extrusion
Zone 5 195 - 220 °C383 - 428 °F
Adapter Temperature 200 - 225 °C392 - 437 °FSheet Extrusion
Die Temperature 195 - 220 °C383 - 428 °FExtrusion Blow Molding
 210 - 240 °C410 - 464 °FSheet Extrusion
Melt Temperature 210 - 225 °C410 - 437 °F
 210 - 240 °C410 - 464 °F
Head Temperature 195 - 220 °C383 - 428 °FZone 7 - Bottom Temperature
 195 - 220 °C383 - 428 °FZone 6 - Top Temperature
Mold Temperature 40.0 - 90.0 °C104 - 194 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FExtrusion Blow Molding
 90.0 - 95.0 °C194 - 203 °FSheet Extrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourSheet Extrusion
 4.00 - 5.00 hour4.00 - 5.00 hourExtrusion Blow Molding
 24.0 hour24.0 hourCumulative; Extrusion Blow Molding
Moisture Content 0.020 - 0.040 %0.020 - 0.040 %
 >= 0.040 %>= 0.040 %
Screw Speed 20 - 60 rpm20 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10013 / 243480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.