MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DAK Americas Laser+® MB912 PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient processing and good overall bottle properties. This polymer is formulate to provide improved efficiencies in perform and bottle production while delivering a robust processing window. Bottles made with Laser+® MB912 deliver good CO2 barrier with continued excellent performance in creep and environmental stress-crack resistance.

Key Attributes:

  • Good performance in stress-crack resistance
  • High reheat capability that provides fast and efficient processing in stretch blow molding
  • Good CO2 barrier
  • Robust processing window

Application/Uses: Carbonated soft drink bottles and custom, edible oil, food, juices and personal care bottles and containers.

Information provided by DAK Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.817 g/cc0.0295 lb/in³Poured; ASTM D1895
 0.881 g/cc0.0318 lb/in³Vibrated; ASTM D1895
Density 1.40 g/cc0.0506 lb/in³Crystalline; ASTM D1505
Melt Density 1.20 g/cc
@Temperature 285 °C
0.0434 lb/in³
@Temperature 545 °F
ASTM D1238
Particle Size 2500 µm2500 µmCubical Shape
Viscosity Test 82 - 86 cm³/g0.82 - 0.86 dl/gIntrinsic; DRAM-A-G-V-3
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 59.0 J/g25.4 BTU/lbDSC on the first heating cycle; ASTM E793
Specific Heat Capacity  1.00 J/g-°C
@Temperature 22.8 °C
0.240 BTU/lb-°F
@Temperature 73.0 °F
ASTM E1269
 1.21 J/g-°C
@Temperature 80.0 °C
0.290 BTU/lb-°F
@Temperature 176 °F
ASTM E1269
 1.38 J/g-°C
@Temperature 100 °C
0.330 BTU/lb-°F
@Temperature 212 °F
ASTM E1269
 1.72 J/g-°C
@Temperature 200 °C
0.410 BTU/lb-°F
@Temperature 392 °F
ASTM E1269
 1.88 J/g-°C
@Temperature 280 °C
0.450 BTU/lb-°F
@Temperature 536 °F
ASTM E1269
Crystallization Temperature 245 °C473 °FDSC on second heating cycle, Peak Melting Point; ASTM D3418
 
Descriptive Properties
Color>74.5 CIEL*, DRAM-A-G-RS-1
 -4 - -1 CIEb*, DRAM-A-G-RS-1
Compounds<3 ppmAcetaldehyde, DRAM-A-G-GC-5
Fines<0.05%DRAM-A-GA-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SABIC BC 112 Crystalline Polyethylene Terephthalate
Eastman BD445 PET
Eastman CB12 PET
Axiall 6741 Moldings & Extrusions Flexible PVC
BLUESTAR PBT 6630 30% Glass Filled

PDAKA002 / 147977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.