MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mapal Plastics Maplon Type 3G Polypropylene Sheet
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Maplon type “3G” is a single layer highly polished clear sheets, with anti-blocking properties.

Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Suitable to offset printing with UV or Oxidation inks and can use when food contact needed
Main disadvantages: Low scratch resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/cc
Thickness 500 microns19.7 mil
Surface Tension >= 48 dynes/cm>= 48 dynes/cmAfter 2 months from production
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
ASTM D638
Film Tensile Strength at Yield, TD 29.0 MPa
@Temperature 23.0 °C
4210 psi
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, MD >= 600 %
@Temperature 23.0 °C
>= 600 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, TD >= 600 %
@Temperature 23.0 °C
>= 600 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, MD 24 %
@Temperature 23.0 °C
24 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, TD 23 %
@Temperature 23.0 °C
23 %
@Temperature 73.4 °F
ASTM D638
Modulus of Elasticity 0.280 GPa
@Temperature 23.0 °C
40.6 ksi
@Temperature 73.4 °F
MD/TD; ASTM D638
Tear Strength <= 130 kN/m<= 742 pliMapal internal
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 136 °C277 °FASTM D1525
Heat Distortion Temperature 79.0 °C174 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze <= 11 %
@Thickness 0.500 mm
<= 11 %
@Thickness 0.0197 in
Sheet
Gloss >= 110 %>= 110 %60°; ASTM D523
Transmission, Visible >= 98 %>= 98 %Depends on thickness
 
Descriptive Properties
ColorTransparent, slightly yellow in bulk

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Changzhou Jinlibao GETAILONG JLB-110802 Matte APET sheet
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
Corning Willow® Flexible Display Glass
Excelite Plastic Polycarbonate solid sheet
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet

PMAPAL04 / 83615

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.