MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T S40000 Series Stainless Steel

Material Notes:

Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.

Information provided by Allegheny Ludlum

Key Words: UNS S40300
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.64 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B <= 96<= 96Annealed
 93 - 10093 - 100Hardened and Tempered
Tensile Strength, Ultimate >= 483 MPa>= 70100 psiAnnealed
 >= 689 MPa>= 99900 psiHardened and Tempered
Tensile Strength, Yield >= 207 MPa>= 30000 psiAnnealed
 >= 483 MPa>= 70100 psiHardened and Tempered
Elongation at Break >= 18 %>= 18 %Hardened and Tempered
 >= 25 %>= 25 %Annealed
 >= 20 %
@Thickness <=12.7 mm
>= 20 %
@Thickness <=0.500 in
Annealed
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000570 ohm-cm
@Temperature 20.0 °C
0.0000570 ohm-cm
@Temperature 68.0 °F
 0.0000640 ohm-cm
@Temperature 100 °C
0.0000640 ohm-cm
@Temperature 212 °F
 0.0000720 ohm-cm
@Temperature 200 °C
0.0000720 ohm-cm
@Temperature 392 °F
 0.0000880 ohm-cm
@Temperature 400 °C
0.0000880 ohm-cm
@Temperature 752 °F
 0.0001035 ohm-cm
@Temperature 600 °C
0.0001035 ohm-cm
@Temperature 1110 °F
 0.000111 ohm-cm
@Temperature 700 °C
0.000111 ohm-cm
@Temperature 1290 °F
Magnetic Permeability 900900Maximum for annealed alloy. Alloy is ferromagnetic in all conditions.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.90 µm/m-°C
@Temperature 20.0 - 100 °C
5.50 µin/in-°F
@Temperature 68.0 - 212 °F
 11.2 µm/m-°C
@Temperature 20.0 - 500 °C
6.22 µin/in-°F
@Temperature 68.0 - 932 °F
 11.9 µm/m-°C
@Temperature 20.0 - 787 °C
6.61 µin/in-°F
@Temperature 68.0 - 1450 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  25.0 W/m-K
@Temperature 100 °C
174 BTU-in/hr-ft²-°F
@Temperature 212 °F
 28.8 W/m-K
@Temperature 500 °C
200 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1495 °C2723 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 11.5 - 13 %11.5 - 13 %
Iron, Fe >= 84.68 %>= 84.68 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni <= 0.60 %<= 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 80-60-03
AISI 403 12Cr STAINLESS STEEL BARS FOR TURBINE BLADES (SUS 403-B)
Ductile Iron grade 60-40-18
AISI 1017 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1017 Steel, cold drawn

NL1017 / 17785

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.