MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Quantum Composites QC-2150 50% Glass Reinforced Phenolic SMC
Categories: Polymer; Thermoset; Composite SMC; Phenolic; Phenolic/Glass Fiber SMC

Material Notes: QC-2150 is a glass reinforced phenolic engineered structural composite molding compound. It exhibits outstanding low flammability characteristics. QC-2150 is recommended for applications such as aircraft interiors and public transportation components requiring composite materials having very low flammability, low smoke, and minimal generation of toxic gasses.

  • Form = Rolled Sheet
  • Color = Natural, Black
  • Glass Fiber Content = 50% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.82 g/cc1.82 g/ccASTM D792
Linear Mold Shrinkage 0.0015 cm/cm0.0015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 227 MPa32900 psiASTM D638
Flexural Strength 358 MPa51900 psiASTM D790
Flexural Modulus 21.0 GPa3050 ksiASTM D790
Izod Impact, Notched 6.40 J/cm12.0 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Shelf Life  2.00 Month
@Temperature 4.44 °C
2.00 Month
@Temperature 40.0 °F
 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fiber Length (in)1Glass, nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-3 Fiberglass Phenolic Laminate Sheet
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
Phenolic 27%, Graphite fabric 73%
Overview of materials for Phenolic; Unreinforced; Molded
Overview of materials for Phenolic/Glass Fiber SMC

PCOQB911 / 139279

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.