MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sylvania SX199 Tungsten & Chrome Based Thermal Spray Powder
Categories: Ceramic; Carbide; Metal; Nonferrous Metal; Tungsten Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SX199 is a premium grade, pre-alloyed tungsten carbide/chromium carbide/tungsten/nickel-chromium powder. The particles are dense, spherical, free flowing and can be applied by plasma or high velocity thermal spray processes. This working composition can be used for wear resistance in oxidizing atmospheres up to 1000°F.

Applications

  • Seal and bearings for process fluid pumps
  • Cutters for food processing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 4.70 - 5.60 g/cc0.170 - 0.202 lb/in³
Particle Size <= 2.0 µm<= 2.0 µm2 wt% max; ASTM B822
 <= 16 µm<= 16 µm12 wt% max; ASTM B822
Particle Mesh Size 270 Mesh270 Mesh1% bigger
 325 Mesh325 Mesh75% smaller
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 5.5 - 6.5 %5.5 - 6.5 %
Chromium, Cr 21 - 25 %21 - 25 %
Nickel, Ni 5.0 - 8.0 %5.0 - 8.0 %
Tungsten, W 60.5 - 68.5 %60.5 - 68.5 %
 
Descriptive Properties
Hall Flow, seconds/50g8-20ASTM B213

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
Sylvania SA201 Tungsten & Chrome Based Thermal Spray Powder
Sylvania SX195 Chrome Based Thermal Spray Powder
Sylvania SX427 Tungsten & Chrome Based Thermal Spray Powder
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy

CSYLV20 / 2319

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.