Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and is easy to process. Applications: dashboards, door panels and pockets, window frames, center consoles, and other automotive interior parts.Information provided by Borealis AG |