MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin POLYFLON™ PTFE M-111 Polytetrafluoroethylene Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: DAIKIN-POLYFLON PTFE (polytetrafluoroethylene) molding powders are well suited for a variety of demanding chemical, mechanical, electrical and non-stick surface applications. These fully fluorinated have excellent thermal, electrical, and chemical properties, with a continuous service rating of 500°F (260°C). DAIKIN-POLYFLON PTFE molding powders are available in homopolymer and modified fine cut grades.

Daikin PTFE molding powders can be used continuously at temperatures up to 260°C (500°F) and for short periods of time at higher temperatures. They also possess excellent low temperature strength.

Daikin PTFE molding powders are completely inert to attack by all chemicals except high temperature, high-pressure elemental fluorine gas, molten alkaline metals and chlorine trifluoride.

The non-polar molecular structure makes Daikin PTFE molding powders ideal for use as high frequency insulating material. The dielectric constant and dissipation factor are uniformly low over a wide frequency range.

Low Friction: Under ordinary conditions of use, Daikin PTFE molding powders possess the lowest coefficient of friction of any solid material. Also, the non-stick properties of these products prevent most materials from adhering to them.

Typical Applications: Chemical/Mechanical—Packings, gaskets, diaphragms, bellows, corrosion-resistant linings, piping components, pump parts, O-rings, V-rings, bushings, slide bearings, etc. Electrical/Other—Insulating skived tape, insulating sleeves, terminals, connectors, sockets, spacers, electronic parts, laboratory equipment, etc.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.17 g/cc2.17 g/ccASTM D 4894
Bulk Density >= 0.360 g/cc>= 0.0130 lb/in³ASTM D 4894
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiASTM D 4894
Elongation at Break 500 %500 %ASTM D 4894
Compressive Yield Strength 8.70 MPa1260 psi0.2% offset; ASTM D695
 5.90 MPa
@Strain 1 %
856 psi
@Strain 1 %
ASTM D695
 28.6 MPa
@Strain 25 %
4150 psi
@Strain 25 %
ASTM D695
Compression Set  3.0 %
@Pressure 13.7 MPa,
Time 90000 sec
3.0 %
@Pressure 1990 psi,
Time 25.0 hour
ASTM D621
 4.1 %
@Pressure 6.90 MPa,
Time 720000 sec
4.1 %
@Pressure 1000 psi,
Time 200 hour
ASTM D621
 7.4 %
@Pressure 13.7 MPa,
Time 360000 sec
7.4 %
@Pressure 1990 psi,
Time 100 hour
ASTM D621
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant <= 2.1
@Frequency 1000 Hz
<= 2.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 135 kV/mm
@Thickness 0.100 mm
3430 kV/in
@Thickness 0.00394 in
Dielectric Loss Index <= 0.00010
@Frequency 1000 Hz
<= 0.00010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 324 °C615 °F
Maximum Service Temperature, Air 260 °C500 °F
Shrinkage 4.4 %4.4 %ASTM D4894
 
Descriptive Properties
MIT Flex3,000,000 cyclesASTM D2178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE 7A Granular Molding Powder
Daikin POLYFLON™ PTFE M-112 Polytetrafluoroethylene Molding Powder
Daikin POLYFLON F-201 PTFE Fine Powder
3M Dyneon™ TF 1750 PTFE
Shamrock Technologies NanoFLON® P 63B Thermoplastic Grade PTFE Additive

PDAIJ9878 / 209949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.