MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carmel Olefins 1018 CAPILENE® QL 55 H Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: CAPILENE® QL 55 H is a polypropylene random copolymer with a high ethylene content, developed for sealing layers in coextruded Cast and Bioriented metalized films

Information provided by Carmel Olefins Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 5.00 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.00 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 19.0 MPa2760 psiISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPa2610 psiISO 527-3
Tensile Strength, Yield 20.0 MPa
@Thickness 50.0 mm,
Time 60.0 sec
2900 psi
@Thickness 1.97 in,
Time 0.0167 hour
ISO 527-2
Elongation at Yield 16.0 %
@Time 60.0 sec
16.0 %
@Time 0.0167 hour
in 50 mm; ISO 527-2
Flexural Modulus 0.600 GPa
@Thickness 5.00 mm,
Time 60.0 sec
87.0 ksi
@Thickness 0.197 in,
Time 0.0167 hour
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Dart Drop Test 400 g0.882 lbF 50; ISO 7765-A
Film Tensile Strength at Break, MD 600 MPa87000 psiISO 527-3
Film Tensile Strength at Break, TD 500 MPa72500 psiISO 527-3
Heat Seal Strength Initiation Temperature 117 °C
@Load 0.100 kg,
Thickness 10.0 mm
243 °F
@Load 0.221 lb,
Thickness 0.394 in
Internal Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 137 °C279 °FASTM D3417
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FISO 75-2
Vicat Softening Point 120 °C248 °F10 N; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze 1.00 %1.00 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARM718 / 327003

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.