MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Kunststoffe AUROform® H03 black POM-Homopolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Product description: AUROform® H03 black is a regranulated POM-Homopolymer injection molding grade with high rigidity, hardness, toughness and high viscosity

Typical applications: Gear wheels, locking devices, technical housings, furniture fixtures

Information provided by Aurora Kunststoffe GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %50% r.h.; ISO 62
Water Absorption at Saturation 0.90 %0.90 %Water; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Temperature 80.0 °C
0.022 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm
@Temperature 80.0 °C
0.019 in/in
@Temperature 176 °F
60x60x2, MT; ISO 294-4
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 65.0 MPa9430 psi50mm/min; ISO 527-1,-2
Elongation at Break 40 %40 %50mm/min; ISO 527-1,-2
Tensile Modulus 2.80 GPa406 ksi1mm/min; ISO 527-1,-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eA
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 176 °C349 °FISO 11357-1,-3
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75,-1,-2
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 °C401 °F
Mold Temperature 90.0 °C194 °F
Drying Temperature 100 °C212 °F
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hour
Moisture Content <= 0.020 %<= 0.020 %Residual, Karl Fischer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAUROK040 / 249734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.