MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Arnite® T06 204 XL PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Low Viscosity, Injection Molding, Low outgassing

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Water Absorption 0.45 %0.45 %Sim. To ISO 62
Moisture Absorption 0.180 %0.180 %Sim. To ISO 62
Viscosity  8000 cP
@Shear Rate 100000 1/s,
Temperature 270 °C
8000 cP
@Shear Rate 100000 1/s,
Temperature 518 °F
 8500 cP
@Shear Rate 100000 1/s,
Temperature 250 °C
8500 cP
@Shear Rate 100000 1/s,
Temperature 482 °F
 9000 cP
@Shear Rate 100000 1/s,
Temperature 230 °C
9000 cP
@Shear Rate 100000 1/s,
Temperature 446 °F
 100000 cP
@Shear Rate 1 1/s,
Temperature 270 °C
100000 cP
@Shear Rate 1 1/s,
Temperature 518 °F
 175000 cP
@Shear Rate 1 1/s,
Temperature 250 °C
175000 cP
@Shear Rate 1 1/s,
Temperature 482 °F
 300000 cP
@Shear Rate 1 1/s,
Temperature 230 °C
300000 cP
@Shear Rate 1 1/s,
Temperature 446 °F
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inSim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm0.020 in/inSim. To ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psiISO 527-1/-2
Elongation at Break 12 %12 %ISO 527-1/-2
Elongation at Yield 8.5 %8.5 %ISO 527-1/-2
Tensile Modulus 2.70 GPa392 ksiISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant  3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
 3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 170 °C338 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC60695-11-10
 HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 570 NC000 POM-GF20
Aclo Accucomp PET PET008L
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
INEOS Styrolution Luran® S KR 2867 C WU Colored ASA+PC
BASF Ultramid® 66 H2 G/25-V0KB1 BK 3324 PA66 (Dry)

PDSM9784 / 161405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.