MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 60% Glass Fiber Filled

Material Notes: Description: Ultramid HMG14 HS BK-102 is a 60% glass reinforced, injection molding grade of PA66 offering high strength and stiffness. Due to inherently lower moisture absorption, Ultramid HMG14 HS BK-102 shows improved retention of mechanical properties after moisture conditioning. In addition, molded parts possess an exceptional surface finish.

Applications: Ultramid HMG14 HS BK-102 was designed for applications requiring very high rigidity and should be considered for components that are constructed with metal.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 248 MPa36000 psiISO 527
Elongation at Break 2.2 %2.2 %ISO 527
Tensile Modulus 20.2 GPa2930 ksiISO 527
Flexural Strength 383 MPa55500 psiISO 178
Flexural Modulus 18.9 GPa2740 ksiISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²ISO 180
 13.0 kJ/m²6.19 ft-lb/in²ISO 180
Charpy Impact Unnotched  9.50 J/cm²
@Temperature -30.0 °C
45.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 9.90 J/cm²
@Temperature 23.0 °C
47.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 224 °C435 °FISO 75
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 305 °C536 - 581 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Dry Time 2 - 4 hour2 - 4 hour
Moisture Content <= 0.12 %<= 0.12 %
 
Descriptive Properties
ColorBK 102
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® HMG14 HS BK 102 60% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)

PBASG0461 / 132094

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.