MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Plenco 1530 Polyester, Briquette, Injection Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stability. UL recognized under component file E40654. 01530 is available in black, grey, or blue color.

Information supplied by Plenco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.870 g/cc0.0314 lb/in³ASTM D1895
Density 1.99 g/cc0.0719 lb/in³ASTM D792
Water Absorption 0.132 %0.132 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 7878ASTM D785
Tensile Strength, Ultimate 82.0 MPa11900 psiASTM D638
Elongation at Break 0.59 %0.59 %ASTM D638
Tensile Modulus 20.2 GPa2930 ksiASTM D638
Flexural Strength 135 MPa19600 psiASTM D790
Flexural Modulus 17.7 GPa2570 ksiASTM D790
Compressive Strength 166 MPa24100 psiASTM D695
Poissons Ratio 0.300.30ASTM D638
Shear Modulus 7.77 GPa1130 ksiCalculated
Izod Impact, Notched 0.340 J/cm0.637 ft-lb/inASTM D256
Charpy Impact, Notched 0.271 J/cm²1.29 ft-lb/in²ASTM D256
Impact 200200J/m Drop Ball Impact; PLENCO
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmASTM D247
Dielectric Constant 4.64.6ASTM D150
Dielectric Strength 11.7 kV/mm297 kV/inStep by Step; ASTM D149
 15.0 kV/mm381 kV/inShort Time; ASTM D149
Dielectric Breakdown 23000 V23000 V1hr 120C; ASTM D149
Dissipation Factor 0.01590.0159ASTM D150
Arc Resistance 190 sec190 secASTM D495
Comparative Tracking Index 600 V600 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear 43.0 µm/m-°C
@Temperature 40.0 - 130 °C
23.9 µin/in-°F
@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.720 W/m-K
@Temperature 100 °C
5.00 BTU-in/hr-ft²-°F
@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 220 °C428 °FHeat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 261 °C502 °FASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
Oxygen Index 25 %25 %ASTM D2863
Shrinkage 0.0115 %0.0115 %72 hr, 120ºC; ASTM D1299

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plenco 1501 Polyester, Briquette, Transfer Molded
Plenco 1581 Polyester, Pellet, Injection Molded
Plenco 1586 Polyester, Pellet, Injection Molded
Plenco 1501 Polyester, Pellet, Injection Molded
Plenco 1500 Polyester, Granular, Transfer Molded

PLEL23 / 50591

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.