Data provided by the manufacturer, ComAlloy International Company. 40% Glass/Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materials The ComAlloy product line has been integrated into the A Schulman product line. |
Polyamide 6/6; Polyamide 66; Nylon 66; ComAlloy International Company, subsidiary of A. Shulman Inc. |