MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 205G FR HS  Nylon 4/6 (PA 4/6) Glass Fiber 30% - Flame Retardant - Heat Stable  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Flame Retarded + Glass Fiber Reinforced

Material Notes: Glass Fiber 30% - Flame Retardant - Heat Stable

Comments:

  • Glass Fiber
  • Flame Retardant
  • Heat Stabilized

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.

This product has been discontinued, please contact RTP Company regarding alternate grades.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.66 g/cc1.66 g/ccASTM D792
Filler Content 30 %30 %
Water Absorption 0.90 %0.90 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage  0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 0.0050 cm/cm
@Thickness 6.35 mm
0.0050 in/in
@Thickness 0.250 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Ultimate 172 MPa25000 psiASTM D638
Elongation at Break 2.0 - 4.0 %2.0 - 4.0 %ASTM D638
Modulus of Elasticity 12.1 GPa1750 ksiASTM D638
Flexural Yield Strength 241 MPa35000 psiASTM D790
Flexural Modulus 10.3 GPa1500 ksiASTM D790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.17 mm
1.50 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.7937 mm
V-0
@Thickness 0.03125 in
Per testing by RTP Company; ASTM D3801
 
Processing PropertiesMetricEnglishComments
Processing Temperature 293 - 321 °C560 - 610 °F
Mold Temperature 79.4 - 149 °C175 - 300 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi
 
Descriptive Properties
ColorNatural

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Techmer ES HiFill® PA4/6 GF30 TL15 30% Glass Filled
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
Mitsui Arlen™ PA46 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
Envalior Stanyl® 46HF5040 PA46-GF40 FR(17), Dry, 40% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Stanyl® 46HF4130 PA46-GF30, Conditioned, 30% Glass Filled, Heat Stabilized

PR5805 / 65206

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.