MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Incronibsi™ Mac-Incronibsi™14-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Solder/Braze Alloy

Material Notes: Melt-Spun Foil is produced by a rapid solidification technique. The flexible foils of brittle alloys that are made this way cannot be formed by conventional hot or cold rolling. High-purity Melt-Spun Foil alloy of nickel, chromium, silicon, boron and iron, for vacuum brazing.

Applications:

  • Heat exchanger assemblies
  • Aero engine compressor vanes, stators and hush kits
  • Bonding diamond compounds to tungsten carbide cutting tools

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.47 g/cc0.270 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 960 - 1090 °C1760 - 1990 °F
Solidus 960 °C1760 °F
Liquidus 1094 °C2001 °F
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.2 %3.2 %nominal
Iron, Fe 4.5 %4.5 %nominal
Nickel, Ni 73.8 %73.8 %nominal
Silicon, Si 4.5 %4.5 %nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alloy 19® Thermocouple Alloy
Morgan Advanced Ceramics Cusil™ Mac-Cusil™-WM Braze Alloy
China Tungsten YG6A Tungsten Carbide for Cutting Tools
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics Nicusil™ Mac-Nicusil™ 8-WM Braze Alloy

CMORF8010 / 203487

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.