MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Low brass, UNS C24000, OSO70 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Excellent cold workability; good hot formability.

The Romans called this alloy "orichalcum", which also contained trace amounts of lead, tin, and other metals and was used to strike coins. Orichalcum is also the name of a naturally occurring gold-copper alloy that is only found in the Andes Mountains of South America.

Applications: battery caps, bellows, musical instruments, clock dials, pump lines, flexible hose.

Test specimen: flat products - 1mm thickness.

Key Words: 80/20 brass, pump lines, flexible hose, flat products, wire, Low brass, UNS C24000, CZ103, ISO CuZn20, CEN CW503L, gilding metal, 80/20 brass, orichalcum
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.67 g/cc0.313 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 5757
Hardness, Rockwell 30T 8.08.0
Tensile Strength, Ultimate 290 MPa42100 psi
Tensile Strength, Yield 83.0 MPa12000 psi
Elongation at Break 52 %52 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksi
Poissons Ratio 0.3750.375
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 40.0 GPa5800 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000539 ohm-cm0.00000539 ohm-cm
Magnetic Susceptibility -1.00e-6-1.00e-6Approximately, cgs units
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.1 µm/m-°C
@Temperature 20.0 - 300 °C
10.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 140 W/m-K
@Temperature 20.0 °C
972 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 965 - 1000 °C1770 - 1830 °F
Solidus 965 °C1770 °F
Liquidus 1000 °C1830 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 700 °C797 - 1290 °F
Hot-Working Temperature 825 - 900 °C1520 - 1650 °F
Recrystallization Temperature 400 °C752 °FApproximately, for 37% reduction and 0.06mm initial grain size
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 78.5 - 81.5 %78.5 - 81.5 %
Iron, Fe >= 0.050 %>= 0.050 %
Lead, Pb >= 0.050 %>= 0.050 %
Zinc, Zn 20 %20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cartridge Brass, UNS C26000 (260 Brass), OS100 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO70 Temper flat products
Overview of materials for Brass
Copper, UNS C26800 (Yellow brass), OSO70 Temper flat products
Low-leaded brass, UNS C33500, OSO70 Temper flat products

MC24000b2 / 11056

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.