MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Acrylonitrile Butadiene Styrene

Flame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistance

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D 792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D 955
Melt Flow 25 g/10 min
@Load 10.0 kg,
Temperature 220 °C
25 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 30.0 MPa4350 psiASTM D 638
Tensile Strength, Yield 40.0 MPa5800 psiASTM D 638
Elongation at Break 5.0 %5.0 %ASTM D 638
Flexural Modulus 2.50 GPa363 ksiASTM D 790
Izod Impact, Notched  0.900 J/cm
@Temperature 0.000 °C
1.69 ft-lb/in
@Temperature 32.0 °F
ASTM D 638
 1.10 J/cm
@Temperature 23.0 °C
2.06 ft-lb/in
@Temperature 73.4 °F
ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point  94.0 °C
@Load 5.00 kg
201 °F
@Load 11.0 lb
50°C/hr; ASTM D 1525
 104 °C
@Load 0.999 kg
219 °F
@Load 2.20 lb
50°C/hr; ASTM D 1525
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
Glow Wire Test 960 °C1760 °FI.E.C. 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® VE-0860EX ABS, Unreinforced FR
Lotte Advanced Materials Starex® VE-0860 ABS, Unreinforced FR
Lotte Advanced Materials Starex® VE-0857 ABS, Unreinforced FR
Lotte Advanced Materials Starex® VE-0855YS ABS, Unreinforced FR
Lotte Advanced Materials Starex® VE-0558 ABS, Unreinforced FR

PCOSSA893 / 156483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.