MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Polyplastics TOPAS® 5013F-04 Cyclic Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: TOPAS® 5013F-04 is a high temperature film extrusion grade for blends. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and healthcare applications. It is used in monolayer cast blends, and in coextruded blends in both cast and blown processes, for a wide variety of film and sheet products requiring excellent optics in applications such as heat resistant blister, hot fill, and easy tear packaging.

Key applications and attributes

  • Pharmaceutical blisters: Clarity, forming, barrier, purity, halogen-free
  • Decorative film and sheet: Gloss, hardness, chemical resistance, forming
  • Food packaging: Hot-fill, easy or linear tear, purity and gloss
  • Healthcare and food: Broad regulatory approval

Information provided by Polyplastics USA, which merged with TOPAS Advanced Polymers in 2018.

Key Words: Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 5.42 g mil/ (m2 day)
@Temperature 38.0 °C
0.350 g mil/ (100 in2 day)
@Temperature 100 °F
90% RH; 1 mil nominal thickness; ISO 15106-3
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption at Saturation 0.010 %
@Temperature 23.0 °C
0.010 %
@Temperature 73.4 °F
ISO 62
Thickness 70.0 microns2.76 milFilm
Melt Flow  <= 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 8.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 1.4 %1.4 %ISO 527-3
Film Elongation at Break, TD 1.1 %1.1 %ISO 527-3
Tensile Modulus 2.50 GPa363 ksiFilm, TD; ISO 527-3
 2.60 GPa377 ksiFilm, MD; ISO 527-3
Elmendorf Tear Strength MD 11 g11 gISO 6383-2
Elmendorf Tear Strength TD 11 g11 gISO 6383-2
Dart Drop Test <= 36.0 g<= 0.0794 lbF50; ISO 7765-1
Film Tensile Strength at Break, MD 35.0 MPa5080 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 134 °C273 °F10°C/min; ISO 11357-1,-2,-3
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %Film; ISO 14782
Gloss >= 100 %>= 100 %60°, Film; ISO 2813
 
Descriptive Properties
Type of film extrusionCastTest specimen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
Polyplastics TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)

POTOPAS06a / 142639

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.