MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei XYRON™ WG720 Polyphenylene Ether + PS, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Glass Filler

Material Notes: Product Description: Modified PPE; 20% Filler reinforced Non-Flame retardant; Please contact us for drinking water standards information

Availability: Africa & Middle East; Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber, 20% Filler by Weight

Features: Drinking Water Contact Acceptable

Processing Method: Injection Molding

Part Marking Code (ISO 11469): PPE+PS-GF20

Information provided by Asahi Kasei Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Water Absorption 0.060 %
@Time 86400 sec
0.060 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0026 - 0.0054 cm/cm
@Thickness 2.00 mm
0.0026 - 0.0054 in/in
@Thickness 0.0787 in
150x150x2 mm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 105 MPa15200 psiISO 527
Elongation at Break 2.0 %2.0 %ISO 527
Flexural Strength 164 MPa23800 psiISO 178
Flexural Modulus 6.50 GPa943 ksiISO 178
Charpy Impact, Notched 1.01 J/cm²
@Thickness 4.00 mm
4.80 ft-lb/in²
@Thickness 0.157 in
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.1
@Frequency 100 Hz
3.1
@Frequency 100 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.00060
@Frequency 100 Hz
0.00060
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 27.0 µm/m-°C
@Temperature -30.0 - 65.0 °C
15.0 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.4 µm/m-°C
@Temperature -30.0 - 65.0 °C
38.0 µin/in-°F
@Temperature -22.0 - 149 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 136 °C277 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 300 °C500 - 572 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASAHJ018 / 310711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.