MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Asahi Kasei Stylac™ 920 ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Flame Retardant: Halogen

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 59 g/10 min
@Load 9.99 kg,
Temperature 220 °C
59 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 101101ISO 2039-2
Tensile Strength, Yield 44.0 MPa6380 psi50mm/min; ISO 527-1
Flexural Strength 70.0 MPa10200 psi2mm/min; ISO 178
Flexural Modulus 2.55 GPa370 ksi2mm/min; ISO 178
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 - 100 µm/m-°C38.9 - 55.6 µin/in-°FASTM D696
Maximum Service Temperature, Air 50.0 °C122 °FRelative Thermal Index; UL 746A
Hot Ball Pressure Test 80.0 °C176 °FEMAC
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C165 °FISO 75-1,2
Vicat Softening Point 88.0 °C
@Load 5.10 kg
190 °F
@Load 11.2 lb
ISO 306
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 2.50 mm
5VA
@Thickness 0.0984 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Asahi Kasei Stylac™ 190 ABS Polymer, High Flow
Asahi Kasei Stylac™ 321 ABS Polymer, High Impact
Bamberger Polymers Bapolene® 1072 Polyethylene, Injection Grade
Chi Mei Polylac® PA-758 ABS - Transparent

PASAHI8301 / 221325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.