MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Daploy WB130HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is generally characterized by improved processability in polymer forming technologies where stretching flows occur.

Daploy WB130HMS has been developed for thermoformable, foamed films and sheets, lightweight packaging trays, beakers and containers, microwaveable food packaging, technical foams for automotive applications such as headliners, carpet backing, door liners, parcel shelves, water shields, under-the-hood acoustic panels, cushioning and protective packaging, and thermal and acoustic insulation.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.00 MPa5801 psiISO 527-2
Elongation at Yield 6.0 %6.0 %ISO 527-2
Tensile Modulus 2.00 GPa290 ksiISO 527-2
Flexural Modulus 1.90 GPa276 ksiISO 178
Charpy Impact Unnotched 100 J/cm²476 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179/1eA
 0.100 J/cm²
@Temperature -20.0 °C
0.476 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature >= 280 °C>= 536 °F
Front Barrel Temperature >= 230 °C>= 446 °F
Die Temperature >= 290 °C>= 554 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion
Borealis Daploy™ WB140HMS Polypropylene
Armacell ArmaFORM® FR150 PET foam core
Borealis Daploy™ WB260HMS Polypropylene
Borealis Daploy™ WF420HMS High Melt Strength Polypropylene for Extrusion Coating

PBOREA170 / 27477

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.