MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Solventless Electrical Varnish

Material Notes: Data provided by Von Roll Isola USA.

Flash Point: 24°C. Average solids: 50%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, bare copper coils, etc. where good adhesion is desired.

Key Words: Von Roll Isola USA; Insulating Materials Incorporated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Viscosity 205 cP205 cP
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 114 kV/mm2900 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 155 °C311 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FSuggested baking time at this temperature is 4-6 hr.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Von Roll Isola IMI Varnish 9637AP Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 707 Solventless Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 704 Solventless Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 702 Solventless Polyester Varnish for Electrical Insulation

PISO24 / 48427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.