MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Carbon Printers FotoDent® Cast Methacrylate resin
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoset; Methacrylate

Material Notes: Purpose: Material based on methacrylate resin for DLP systems with 385 nm/405 nm for the manufacturing of profiles that burn out without any residue for the casting technology.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.20 g/cc0.0397 - 0.0434 lb/in³
Viscosity <= 300 cP<= 300 cP
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 7.5 - 11 %7.5 - 11 %
Flexural Strength >= 100 MPa>= 14500 psi
Flexural Modulus >= 2.00 GPa>= 290 ksi
 
Processing PropertiesMetricEnglishComments
Cure Time 8.00 min0.133 hour+ 1 min gas pre-flow, Post curing time using FotoDent flash
 
Descriptive Properties
ColorRed transparent
Composition1-Methacrylates
 2-Initiators
 3-Pigments

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCARBP001 / 255833

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.