MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

60Ag-40Pd Alloy, Hard
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Key Words: Palladium Silver Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.1 g/cc0.401 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 147147Estimated from Vickers
Hardness, Knoop 171171Estimated from Vickers
Hardness, Rockwell A 4848Estimated from Vickers
Hardness, Rockwell B 8080Estimated from Vickers
Hardness, Vickers 150150
Tensile Strength, Ultimate 440 MPa63800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000210 ohm-cm0.0000210 ohm-cmTemperature Coefficient = 0.0005/K
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.2 µm/m-°C
@Temperature 20.0 - 100 °C
9.00 µin/in-°F
@Temperature 68.0 - 212 °F
 16.8 µm/m-°C
@Temperature 20.0 - 250 °C
9.33 µin/in-°F
@Temperature 68.0 - 482 °F
 17.5 µm/m-°C
@Temperature 20.0 - 500 °C
9.72 µin/in-°F
@Temperature 68.0 - 932 °F
 
Component Elements PropertiesMetricEnglishComments
Palladium, Pd 40 %40 %
Silver, Ag 60 %60 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
60Ag-40Pd Alloy, Annealed
50Ag-50Pd Alloy, Hard
50Ag-50Pd Alloy, Annealed
Cadi 35WS Tungsten Silver
Cadi 20WS Tungsten Silver

MPAgP7 / 12527

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.