MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Palnicro™ Mac-Palnicro™ 30-WM Braze Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Solder/Braze Alloy

Material Notes: High-purity Melt-Spun Foil alloy of nickel, palladium, chromium and boron, for vacuum brazing. Melt-Spun Foil is produced by a rapid solidification technique. The flexible foils of brittle alloys that are made this way cannot be formed by conventional hot or cold rolling.

Applications:

  • Heat exchanger assemblies
  • Aero engine compressor vanes, stators and hush kits
  • Bonding diamond compounds to tungsten carbide cutting tools

information provided by Morgan Advanced Materials

Key Words: Braze Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.41 g/cc0.340 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 941 - 977 °C1730 - 1790 °F
Solidus 941 °C1730 °F
Liquidus 977 °C1790 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Nicoro™ Mac-Nicoro™-WM Braze Alloy
Morgan Advanced Ceramics Nicusil™ Mac-Nicusil™ 3-WM Braze Alloy
Morgan Advanced Ceramics 50Ni-50Cu Mac-50Ni/50Cu-WM Braze Alloy
Morgan Advanced Ceramics Incronibsi™ Mac-Incronibsi™7-WM Braze Alloy
Aluminum 2007-T3

CMORF8015 / 203492

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.