MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Barlog Plastics KEBAPEAK XS2800 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: KEBAPEAK XS 2800 is an unreinforced, high-viscosity PEEK grade that is filtered to achieve particularly high purity. In addition to injection molding applications with high purity requirements, the material is particularly suitable for thin-walled extrusion applications, such as cable sheathing.

Properties: dimensionally stable, good chemical resistance, good gliding properties, good aging behavior, good fire behavior, High wear resistance, Very high continuous used temperature, semi-crystalline

Typical areas of application: Fasteners, Housing, Cable and wire extrusion

Industries: Automotive, Electrical and electronics industry, Household appliances, Aviation Industry, Mechanical Engineering, Medical Technology

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183-1
Water Absorption 0.300 %0.300 %ISO 62
Moisture Absorption 0.0700 %0.0700 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0100 cm/cm0.0100 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0130 cm/cm0.0130 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 85.085.0DIN ISO 7619-1
Tensile Strength at Break 100 MPa14500 psiISO 527-1
Elongation at Break 40.0 %40.0 %ISO 527-1
Modulus of Elasticity 3.50 GPa508 ksiISO 527-1
Charpy Impact Unnotched 10.0 J/cm²47.6 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmContact; IEC 60093
Dielectric Strength 23.0 kV/mm584 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C25.0 µin/in-°FISO 11359-1/-2
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°Fin plane; DIN EN 821
 0.300 W/m-K2.08 BTU-in/hr-ft²-°Fthrough plane; DIN EN 821
Melting Point 343 °C649 °FISO 11357-1/-3
Maximum Service Temperature, Air 240 °C464 °FContinuous; ISO 2578
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FISO 75-1/-2
Glass Transition Temp, Tg 143 °C289 °FDIN EN ISO 11357-1
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FInjection
Melt Temperature 365 - 400 °C689 - 752 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 150 - 160 °C302 - 320 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO683 / 326757

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.