MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Kelon® A FR H2 CET/35-V2 PA 66, 35% Mineral Reinforced, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/in
Linear Mold Shrinkage, Transverse 0.0060 - 0.0075 cm/cm0.0060 - 0.0075 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  20.0 MPa
@Temperature 150 °C
2900 psi
@Temperature 302 °F
 25.0 MPa
@Temperature 120 °C
3630 psi
@Temperature 248 °F
 35.0 MPa
@Temperature 90.0 °C
5080 psi
@Temperature 194 °F
 55.0 MPa
@Temperature 60.0 °C
7980 psi
@Temperature 140 °F
 70.0 MPa
@Temperature 23.0 °C
10200 psi
@Temperature 73.4 °F
Elongation at Break  1.5 %
@Temperature 23.0 °C
1.5 %
@Temperature 73.4 °F
 2.5 %
@Temperature 60.0 °C
2.5 %
@Temperature 140 °F
 7.0 %
@Temperature 90.0 °C
7.0 %
@Temperature 194 °F
 15 %
@Temperature 120 °C
15 %
@Temperature 248 °F
 25 %
@Temperature 190 °C
25 %
@Temperature 374 °F
Elongation at Yield  6.0 %
@Temperature 90.0 °C
6.0 %
@Temperature 194 °F
 10 %
@Temperature 120 °C
10 %
@Temperature 248 °F
 >= 10 %
@Temperature 150 °C
>= 10 %
@Temperature 302 °F
Tensile Modulus  1.60 GPa
@Temperature 150 °C
232 ksi
@Temperature 302 °F
 2.10 GPa
@Temperature 120 °C
305 ksi
@Temperature 248 °F
 3.80 GPa
@Temperature 90.0 °C
551 ksi
@Temperature 194 °F
 7.30 GPa
@Temperature 60.0 °C
1060 ksi
@Temperature 140 °F
 9.50 GPa
@Temperature 23.0 °C
1380 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
 2.50 J/cm²
@Temperature -20.0 °C
11.9 ft-lb/in²
@Temperature -4.00 °F
Charpy Impact, Notched  0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °F
Deflection Temperature at 1.8 MPa (264 psi) 165 °C329 °F
Vicat Softening Point 200 °C
@Load 5.00 kg
392 °F
@Load 11.0 lb
Flammability, UL94  V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Oxygen Index 28 %28 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 200 F SI 2 Nylon 12 (PA) Silicone Lubricated
Nurel Engineering Polymers Promyde® B20 P PA 6, Dry, Heat stabilized, Nucleated and Lubricated
LG Chemical HYPERIER IP1104 PA-PE Nanoclay Compound
Kolon Kopa® KN1331 Nylon 6 Resin
INEOS Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Conditioned)

PLATH9601 / 177297

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.