MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Hyflon® MFA® XPH 5510_1N Perfluoropolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: Hyflon® XPH 5510_1N is a white aqueous MFA dispersion. Hyflon® XPH 5510_1N exhibits excellent wetting properties and high shear stability. Hyflon® XPH 5510_1N has very good film forming behavior and is especially suited for top-coat passes to produce final items with superior gloss. Due to its features, XPH 5510_1N can of course also find use in formulations for coating applications.

Features: High Gloss; Rapid Wetting

Uses: Coating Applications; Impregnation Applications

Additional Properties: Average Particle Size - Internal Method 0.18 µm; Brookfield Viscosity - ASTM D2196 (20°C): 20 mPa·s; MFA Content - ASTM D4441 55.0 wt%; Non Ionic Surfactant - ASTM D4441 3.5 wt%; pH - ASTM D4441 > 9.0

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ASTM D1505
 
Thermal PropertiesMetricEnglishComments
Melting Point 310 °C590 °FDSC
 
Descriptive Properties
AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormLiquid

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y7114 / 176845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.