MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kingfa FRHIPS-301 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes:
    Features:
  • UL 94 V-1 @ 2.0 & 3.2mm
  • Excellent balance properties, high strength
  • Excellent heat stability
  • Excellent electrical properties

    Applications:
  • Injection molding
  • Gas molding
  • TV & Audio housing
  • Electrical appliance housing

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc
@Temperature 23.0 °C
1.18 g/cc
@Temperature 73.4 °F
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Temperature 23.0 °C
0.0040 - 0.0060 in/in
@Temperature 73.4 °F
ASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
10 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 25.0 MPa3630 psi50mm/min; ASTM D638
Elongation at Break 35 %35 %50mm/min; ASTM D638
Flexural Strength 38.0 MPa5510 psi2mm/min; ASTM D790
Flexural Modulus 2.35 GPa341 ksi2mm/min; ASTM D790
Izod Impact, Notched 1.01 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
1.89 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
@Thickness 6.40 mm
174 °F
@Thickness 0.252 in
ASTM D648
Flammability, UL94  V-1
@Thickness 2.00 mm
V-1
@Thickness 0.0787 in
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 250 °C<= 482 °F
Rear Barrel Temperature 182 - 205 °C360 - 401 °FStart Point: 190°C
Middle Barrel Temperature 205 - 230 °C401 - 446 °FStart Point: 215°C
Front Barrel Temperature 215 - 240 °C419 - 464 °FStart Point: 225°C
Melt Temperature 220 - 245 °C428 - 473 °FStart Point: 230°C
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °FStart Point: 50°C
Drying Temperature 70.0 °C
@Time 7200 sec
158 °F
@Time 2.00 hour
Pre-dry
Back Pressure 5.00 - 15.0 MPa725 - 2180 psi
 
Descriptive Properties
Injection SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa PET-RG20 Flame Retardant, 20% Glass Fiber Reinforced PET
Kingfa PET-G30 30% Glass Fiber Reinforced PET
Kingfa PBT-T30 30% Mineral Filled PBT
Kingfa PBT-G30 30% Glass Fiber Reinforced PBT
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose)

PKINGF097 / 104356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.