MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

A. Schulman Premi-Glas® 1281-47 VE SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: Description: Premi-Glas® 1281-47 VE is a sheet molding compound.

Market: Structural

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/cc
Linear Mold Shrinkage 0.00075 cm/cm0.00075 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 140 MPa20300 psiASTM D638
Elongation at Break 1.3 %1.3 %ASTM D638
Tensile Modulus 13.0 GPa1890 ksiASTM D638
Flexural Strength 270 MPa39200 psiASTM D790
Flexural Modulus 14.0 GPa2030 ksiASTM D790
Poissons Ratio 0.330.33
Shear Modulus 4.90 GPa711 ksiCalculated
Izod Impact, Notched 10.0 J/cm18.7 ft-lb/inASTM D256
Izod Impact, Unnotched 17.0 J/cm31.8 ft-lb/inASTM D4812
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 20.0 µm/m-°C11.1 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC
A. Schulman Premi-Glas® 1200-30 Polyester SMC
A. Schulman Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC

PPREMI09 / 58136

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.