MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Zinc Silicon Phosphide, ZnSiP2
Categories: Ceramic; Phosphide/Pnictide; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.39 g/cc0.122 lb/in³
a Lattice Constant 5.40 Å5.40 Å
c Lattice Constant 10.441 Å10.441 Å
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 1100011000N/mm²
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.80e+6 ohm-cm1.80e+6 ohm-cmCVT-grown
Band Gap 2.3 eV2.3 eV
Electron Mobility, cm²/V-s 10001000
 
Thermal PropertiesMetricEnglishComments
Melting Point 1367 °C2493 °F
Heat of Formation 312 kJ/mol312 kJ/mol
Decomposition Temperature 740 °C1360 °FStability limit in flowing oxygen
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 55 %
@Thickness 0.190 mm
55 %
@Thickness 0.00748 in
thick polished crystal
IR Transmittance 55 %
@Thickness 0.190 mm
55 %
@Thickness 0.00748 in
thick polished crystal; cutoff begins 9 µm
 
Descriptive Properties
Crystal StructureTetragonalChalcopyrite Structure - Space Group I(-4)2d

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zinc Silicon Arsenide, ZnSiAs2
Overview of materials for Acrylic, General Purpose, Molded
Tin Selenide, SnSe
Tin (II) Selenide, SnSe
Silicon, Si

DSEN73 / 3082

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.