MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Epoxy, High Temperature
Categories: Polymer; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.990 - 2.26 g/cc0.0358 - 0.0816 lb/in³Average value: 1.26 g/cc Grade Count:33
Volatile Organic Compounds (VOC) Content 0.000 g/l0.000 g/lAverage value: 0.000 g/l Grade Count:4
Particle Size 20.0 - 45.0 µm20.0 - 45.0 µmAverage value: 25.0 µm Grade Count:9
Viscosity 20.0 - 2.50e+6 cP20.0 - 2.50e+6 cPAverage value: 66100 cP Grade Count:62
 150 - 400000 cP
@Temperature 50.0 - 93.3 °C
150 - 400000 cP
@Temperature 122 - 200 °F
Average value: 100000 cP Grade Count:4
Thickness 1.00 - 1270 microns0.0394 - 50.0 milAverage value: 396 microns Grade Count:5
Linear Mold Shrinkage 0.00300 - 0.00340 cm/cm0.00300 - 0.00340 in/inAverage value: 0.00317 cm/cm Grade Count:3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 67.0 - 96.067.0 - 96.0Average value: 82.8 Grade Count:64
 24.0 - 28.0
@Temperature 100 - 149 °C
24.0 - 28.0
@Temperature 212 - 300 °F
Average value: 26.0 Grade Count:1
Tensile Strength, Ultimate 13.8 - 345 MPa2000 - 50000 psiAverage value: 67.5 MPa Grade Count:41
Elongation at Break 1.00 - 50.0 %1.00 - 50.0 %Average value: 7.94 % Grade Count:19
Modulus of Elasticity 1.68 - 5.40 GPa244 - 783 ksiAverage value: 3.08 GPa Grade Count:49
 1.37895 - 1.72369 GPa
@Temperature 149 - 260 °C
200.003 - 250.004 ksi
@Temperature 300 - 500 °F
Average value: 1.72 GPa Grade Count:3
Flexural Yield Strength 8.27 - 569 MPa1200 - 82500 psiAverage value: 119 MPa Grade Count:11
 17.2369 - 20.6843 MPa
@Temperature 260 - 260 °C
2500.00 - 3000.01 psi
@Temperature 500 - 500 °F
Average value: 19.0 MPa Grade Count:2
Compressive Yield Strength 55.2 - 500 MPa8000 - 72500 psiAverage value: 162 MPa Grade Count:26
Shear Strength 4.83 - 46.9 MPa700 - 6800 psiAverage value: 20.0 MPa Grade Count:22
Adhesive Bond Strength 9.65 - 110 MPa1400 - 16000 psiAverage value: 18.3 MPa Grade Count:31
 1.55132 - 14.479 MPa
@Temperature 65.0 - 260 °C
225.000 - 2100.0 psi
@Temperature 149 - 500 °F
Average value: 8.62 MPa Grade Count:5
Peel Strength 0.877 - 1.75 kN/m5.00 - 10.0 pliAverage value: 1.64 kN/m Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 400 - 1.00e+16 ohm-cm400 - 1.00e+16 ohm-cmAverage value: 1.34e+15 ohm-cm Grade Count:55
 1.00e+10 - 1.00e+15 ohm-cm
@Temperature 75.0 - 400 °C
1.00e+10 - 1.00e+15 ohm-cm
@Temperature 167 - 752 °F
Average value: 6.05e+13 ohm-cm Grade Count:10
Dielectric Constant 2.58 - 4.902.58 - 4.90Average value: 3.76 Grade Count:50
 3.20 - 4.80
@Temperature 75.0 - 400 °C
3.20 - 4.80
@Temperature 167 - 752 °F
Average value: 3.84 Grade Count:7
 3.20 - 4.80
@Frequency 60.0 - 1.00e+6 Hz
3.20 - 4.80
@Frequency 60.0 - 1.00e+6 Hz
Average value: 3.84 Grade Count:7
Dielectric Strength 15.6 - 18.9 kV/mm395 - 480 kV/inAverage value: 17.6 kV/mm Grade Count:16
Dissipation Factor 0.000700 - 0.3100.000700 - 0.310Average value: 0.0403 Grade Count:28
 0.00300 - 0.0700
@Temperature 75.0 - 400 °C
0.00300 - 0.0700
@Temperature 167 - 752 °F
Average value: 0.0166 Grade Count:6
 0.00300 - 0.0700
@Frequency 60.0 - 1.00e+6 Hz
0.00300 - 0.0700
@Frequency 60.0 - 1.00e+6 Hz
Average value: 0.0166 Grade Count:6
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 - 231 µm/m-°C9.00 - 128 µin/in-°FAverage value: 82.3 µm/m-°C Grade Count:47
Thermal Conductivity 0.167 - 3.60 W/m-K1.16 - 25.0 BTU-in/hr-ft²-°FAverage value: 1.15 W/m-K Grade Count:20
Maximum Service Temperature, Air 149 - 350 °C300 - 662 °FAverage value: 256 °C Grade Count:80
Minimum Service Temperature, Air -167 - -20.0 °C-269 - -4.00 °FAverage value: -59.0 °C Grade Count:70
Glass Transition Temp, Tg 80.0 - 240 °C176 - 464 °FAverage value: 145 °C Grade Count:39
Decomposition Temperature 341 - 487 °C646 - 909 °FAverage value: 405 °C Grade Count:17
Flash Point 93.3 °C200 °FAverage value: 93.3 °C Grade Count:5
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.52 - 1.621.52 - 1.62Average value: 1.56 Grade Count:11
Transmission, Visible 0.100 - 99.0 %0.100 - 99.0 %Average value: 77.4 % Grade Count:11
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FAverage value: 21.1 °C Grade Count:5
Cure Time 30.0 - 4320 min0.500 - 72.0 hourAverage value: 1220 min Grade Count:32
 1.00 - 1440 min
@Temperature 60.0 - 232 °C
0.0167 - 24.0 hour
@Temperature 140 - 450 °F
Average value: 115 min Grade Count:65
Pot Life 8.00 - 7200 min8.00 - 7200 minAverage value: 1010 min Grade Count:58
 120 - 120 min
@Temperature 80.0 - 80.0 °C
120 - 120 min
@Temperature 176 - 176 °F
Average value: 120 min Grade Count:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Cure Resin
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Overview of materials for Epoxy, Thermally Conductive
Overview of materials for Epoxy/Carbon Fiber Composite

O1712 / 77896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.