Surlyn® 1702 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutical packaging; Powdered/granular food and nonfood pouches; Snack structures Data provided by the manufacturer, DuPont Packaging. This former DuPont product line is now a Dow product line. |
Ethylene/Methacrylic Acid (E/MAA) Copolymer |