MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC CYCOLAC™ INP563 ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Medium flow powder SAN for color concentrates and alloys. FDA compliant (part use must be at room temperature or below).

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Melt Flow  19.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
19.5 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 47 g/10 min
@Load 10.0 kg,
Temperature 220 °C
47 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 123123ASTM D785
Tensile Strength at Break 69.0 MPa10000 psi5 mm/min; ASTM D638
 74.0 MPa10700 psi50 mm/min; ISO 527
Tensile Strength, Yield 69.0 MPa10000 psi5 mm/min; ASTM D638
 74.0 MPa10700 psi50 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %50 mm/min; ISO 527
 2.4 %2.4 %5 mm/min; ASTM D638
Elongation at Yield 2.0 %2.0 %50 mm/min; ISO 527
 2.4 %2.4 %5 mm/min; ASTM D638
Tensile Modulus 3.86 GPa560 ksi5 mm/min; ASTM D638
 3.97 GPa576 ksi1mm/min; ISO 527
Flexural Yield Strength 46.0 MPa6670 psi2 mm/min; ISO 178
 93.0 MPa13500 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.46 GPa502 ksi2 mm/min; ISO 178
 3.77 GPa547 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.180 J/cm0.337 ft-lb/inASTM D256
 0.220 J/cm
@Temperature -30.0 °C
0.412 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²80*10*4; ISO 180/1A
 2.00 kJ/m²
@Temperature -30.0 °C
0.952 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.100 J/cm²0.476 ft-lb/in²ISO 179/2C
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 3.20 mm
203 °F
@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 82.0 °C
@Thickness 3.20 mm
180 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 102 °C216 °FRate B/50; ISO 306
 104 °C219 °FRate B/120; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10061 / 243528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.