MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LGC-4 Precious dental alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 12.1 - 14.1 g/cc0.437 - 0.509 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 155 - 170155 - 170soft
 220 - 275220 - 275hardened
Tensile Strength, Ultimate 480 - 510 MPa69600 - 74000 psisoft
Tensile Strength, Yield 640 - 890 MPa92800 - 129000 psihardened
 310 - 400 MPa
@Strain 0.2 %
45000 - 58000 psi
@Strain 0.2 %
soft
 555 - 830 MPa
@Strain 0.2 %
80500 - 120000 psi
@Strain 0.2 %
hardened
Elongation at Break 3.0 - 13 %3.0 - 13 %hardened
 18 - 43 %18 - 43 %soft
Modulus of Elasticity 94.0 - 106 GPa13600 - 15400 ksi
 
Thermal PropertiesMetricEnglishComments
Melting Point 770 - 1065 °C1420 - 1949 °F
Solidus 770 °C1420 °F
Liquidus 1065 °C1949 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 0.00 - 9.0 %0.00 - 9.0 %
Gold, Au 50 - 73 %50 - 73 %
Indium, In <= 2.0 %<= 2.0 %
Iridium, Ir <= 0.10 %<= 0.10 %
Palladium, Pd <= 1.0 %<= 1.0 %
Platinum, Pt <= 19 %<= 19 %
Rhenium, Re <= 0.10 %<= 0.10 %
Silver, Ag 8.0 - 28 %8.0 - 28 %
Zinc, Zn 6.0 - 14 %6.0 - 14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HGC-4 Precious dental alloy
NAECO® NAECOMET® D154F Pre-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
NAECO® NAECOMET® D154X Post-Oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3
NAECO® NAECOMET® D158F Silver Graphite Contact Material
NAECO® NAECOMET® D355F Pre-oxidized Silver Cadmium Oxide Contact Material ASTM B781 Table 3

MMEDIC38 / 12414

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.