MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Colour Image Plastic Compound FRblend® ABS-1301 ABS, Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Product Description: FRblend® ABS-1301 is an unfilled, halogen-free, flame retardant Acrylonitrile butadiene styrene compound. The flame retardant system is based on non-chlorinated and non-brominated.

Features:

  • good impact resistance
  • Flame retardant
  • Good processability
  • Bromine free
  • Chlorine free
Uses:
  • Hand phones housing
  • Hard disk drives
  • Scanners
  • Laptop housing
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 27 g/10 min
@Load 10.0 kg,
Temperature 220 °C
27 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psiASTM D638
Elongation at Break 14 %14 %ASTM D638
Tensile Modulus 2.547 GPa369.4 ksiASTM D638
Flexural Strength 62.0 MPa8990 psiASTM D790
Flexural Modulus 2.256 GPa327.2 ksiASTM D790
Izod Impact, Notched 1.74 J/cm3.26 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
@Thickness 4.00 mm
176 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 185 - 190 °C365 - 374 °F
Middle Barrel Temperature 190 - 200 °C374 - 392 °F
Front Barrel Temperature 200 - 210 °C392 - 410 °F
Nozzle Temperature 210 - 220 °C410 - 428 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 70.0 - 90.0 °C158 - 194 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO059 / 265951

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.