MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Celanese FORTRON® 9120L4 20% Glass Reinforced Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler

Material Notes: Description: Fortron 9120L4 Natural is a 20% glass fiber reinforced injection molding grade that exhibits excellent heat and chemical resistance, inherent flame retardancy, and high hardness and rigidity at elevated temperatures. Components made from this grade may be used for medical and food handling applications. Fortron 9120L4 is in compliance with ISO 10993, USP Class VI, and is included in the Fortron Drug and Device Master Files at the FDA. These grades comply with FDA Food Contact Notification (FCN 40) for repeat-use applications.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption at Saturation 0.020 %0.020 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ISO 2039-2
Tensile Strength at Break 120 MPa17400 psi5 mm/min; ISO 527-2/1A
Elongation at Break 1.5 %1.5 %5 mm/min; ISO 527-2/1A
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 8.00 GPa1160 ksiISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²16.7 ft-lb/in²ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Fortron® 6165 A4 Polyphenylene Sulfide (PPS), 65% Mineral/Glass-Fiber
Celanese FORTRON® 9320C0 Polyphenylene Sulfide (PPS)
Celanese Fortron® 1130 L4 Polyphenylene Sulfide (PPS), 30% Glass Fiber
Celanese Fortron® 1140 A0 Polyphenylene Sulfide (PPS), 40% Glass Fiber
Celanese FORTRON® 1140 E7 Polyphenylene Sulfide (PPS)

PHCW54 / 45995

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.