MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Vinyl Ester Sheet Molding Compound
Categories: Polymer; Thermoset; Vinyl Ester; Vinyl Ester Sheet Molding Compound

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 - 1.95 g/cc0.0372 - 0.0704 lb/in³Average value: 1.67 g/cc Grade Count:40
Filler Content 30.0 - 60.0 %30.0 - 60.0 %Average value: 48.8 % Grade Count:8
Water Absorption 0.0500 - 0.600 %0.0500 - 0.600 %Average value: 0.257 % Grade Count:23
Linear Mold Shrinkage 0.000 - 0.00120 cm/cm0.000 - 0.00120 in/inAverage value: 0.000645 cm/cm Grade Count:20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 35.0 - 70.035.0 - 70.0Average value: 53.8 Grade Count:15
Tensile Strength, Ultimate 30.3 - 993 MPa4400 - 144000 psiAverage value: 186 MPa Grade Count:39
 58.6054 - 58.6054 MPa
@Temperature 150 - 150 °C
8500.01 - 8500.01 psi
@Temperature 302 - 302 °F
Average value: 58.6 MPa Grade Count:1
Elongation at Break 1.20 - 7.90 %1.20 - 7.90 %Average value: 3.47 % Grade Count:3
Modulus of Elasticity 3.72 - 94.5 GPa540 - 13700 ksiAverage value: 21.8 GPa Grade Count:24
 8.27371 - 8.27371 GPa
@Temperature 150 - 150 °C
1200.02 - 1200.02 ksi
@Temperature 302 - 302 °F
Average value: 8.27 GPa Grade Count:1
Flexural Yield Strength 40.0 - 1310 MPa5800 - 190000 psiAverage value: 298 MPa Grade Count:40
 50.0 - 365 MPa
@Temperature 115 - 150 °C
7250 - 52900 psi
@Temperature 239 - 302 °F
Average value: 179 MPa Grade Count:3
Flexural Modulus 3.45 - 77.9 GPa500 - 11300 ksiAverage value: 18.1 GPa Grade Count:34
 16.2 - 16.2 GPa
@Temperature 115 - 115 °C
2350 - 2350 ksi
@Temperature 239 - 239 °F
Average value: 9.03 GPa Grade Count:1
 6.20528 - 8.27371 GPa
@Temperature 150 - 150 °C
900.014 - 1200.02 ksi
@Temperature 302 - 302 °F
Average value: 9.03 GPa Grade Count:1
 6.20528 - 8.27371 GPa
@Thickness 0.500 - 2.50 mm
900.014 - 1200.02 ksi
@Thickness 0.0197 - 0.0984 in
Average value: 9.03 GPa Grade Count:1
Compressive Yield Strength 103 - 310 MPa15000 - 45000 psiAverage value: 202 MPa Grade Count:17
Compressive Modulus 0.0172 - 33.8 GPa2.49 - 4900 ksiAverage value: 12.2 GPa Grade Count:7
Ultimate Bearing Strength 221 MPa32000 psiAverage value: 221 MPa Grade Count:3
Poissons Ratio 0.305 - 0.3300.305 - 0.330Average value: 0.324 Grade Count:4
Shear Modulus 3.10 - 5.19 GPa450 - 753 ksiAverage value: 4.40 GPa Grade Count:3
Shear Strength 31.0 - 96.5 MPa4500 - 14000 psiAverage value: 49.4 MPa Grade Count:5
Izod Impact, Notched 2.14 - 37.0 J/cm4.00 - 69.3 ft-lb/inAverage value: 10.9 J/cm Grade Count:23
Izod Impact, Unnotched 0.160 - 19.2 J/cm0.300 - 36.0 ft-lb/inAverage value: 12.3 J/cm Grade Count:4
Tensile Impact Strength 12.0 - 62.0 kJ/m²5.71 - 29.5 ft-lb/in²Average value: 40.6 kJ/m² Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0100 - 5.00e+14 ohm-cm0.0100 - 5.00e+14 ohm-cmAverage value: 2.00e+14 ohm-cm Grade Count:4
Dielectric Constant 4.70 - 5.004.70 - 5.00Average value: 4.80 Grade Count:3
Dielectric Strength 1.38 - 20.0 kV/mm35.0 - 508 kV/inAverage value: 10.2 kV/mm Grade Count:14
Arc Resistance 120 - 191 sec120 - 191 secAverage value: 147 sec Grade Count:12
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.00 - 36.0 µm/m-°C4.44 - 20.0 µin/in-°FAverage value: 20.8 µm/m-°C Grade Count:12
CTE, linear, Transverse to Flow 18.0 - 27.0 µm/m-°C10.0 - 15.0 µin/in-°FAverage value: 23.0 µm/m-°C Grade Count:4
Specific Heat Capacity 0.841 - 1.51 J/g-°C0.201 - 0.360 BTU/lb-°FAverage value: 1.28 J/g-°C Grade Count:3
Thermal Conductivity 0.300 - 46.2 W/m-K2.08 - 321 BTU-in/hr-ft²-°FAverage value: 11.1 W/m-K Grade Count:5
 18.5 - 43.7 W/m-K
@Temperature 85.0 - 85.0 °C
128 - 303 BTU-in/hr-ft²-°F
@Temperature 185 - 185 °F
Average value: 31.1 W/m-K Grade Count:1
Maximum Service Temperature, Air 98.0 - 300 °C208 - 572 °FAverage value: 227 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 160 - 271 °C320 - 520 °FAverage value: 217 °C Grade Count:15
Glass Transition Temp, Tg 118 - 200 °C244 - 392 °FAverage value: 165 °C Grade Count:15
Flammability, UL94 HB - V-0HB - V-0Grade Count:10
Flame Spread Index 25.025.0Average value: 25.0 Grade Count:4
Smoke Density 600 - 700600 - 700Average value: 650 Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 93.0 - 160 °C199 - 320 °FAverage value: 139 °C Grade Count:11
Cure Time 0.583333 - 10.0 min
@Temperature 125 - 140 °C
0.00972222 - 0.167 hour
@Temperature 257 - 284 °F
Average value: 1.83 min Grade Count:9
 3.00 - 5.00 min
@Temperature 138 - 138 °C
0.0500 - 0.0833 hour
@Temperature 280 - 280 °F
Average value: 1.83 min Grade Count:1
 3.00 - 5.00 min
@Thickness 6.35 - 6.35 mm
0.0500 - 0.0833 hour
@Thickness 0.250 - 0.250 in
Average value: 1.83 min Grade Count:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Overview of materials for Thermoset Polyester Glass Filled BMC
Applied Composites 175 Vinylester SMC
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles
Overview of materials for Epoxy Cure Resin

O5700 / 78531

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.