MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Mineral Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 - 1.81 g/cc0.0470 - 0.0654 lb/in³Average value: 1.50 g/cc Grade Count:41
Filler Content 25.0 - 30.0 %25.0 - 30.0 %Average value: 26.7 % Grade Count:3
Water Absorption 0.000 - 0.500 %0.000 - 0.500 %Average value: 0.185 % Grade Count:18
Moisture Absorption at Equilibrium 0.150 - 0.500 %0.150 - 0.500 %Average value: 0.275 % Grade Count:6
Water Absorption at Saturation 0.400 - 0.450 %0.400 - 0.450 %Average value: 0.425 % Grade Count:4
Maximum Moisture Content 0.02000.0200Average value: 0.0200 Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm0.00100 - 0.0180 in/inAverage value: 0.0111 cm/cm Grade Count:28
Linear Mold Shrinkage, Transverse 0.00100 - 0.0190 cm/cm0.00100 - 0.0190 in/inAverage value: 0.0119 cm/cm Grade Count:13
Melt Flow 10.0 - 58.0 g/10 min10.0 - 58.0 g/10 minAverage value: 25.3 g/10 min Grade Count:18
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 50.0 - 10450.0 - 104Average value: 77.8 Grade Count:4
Hardness, Rockwell R 109 - 119109 - 119Average value: 114 Grade Count:7
Tensile Strength, Ultimate 45.0 - 185 MPa6530 - 26800 psiAverage value: 63.4 MPa Grade Count:28
 35.0 - 55.0 MPa
@Temperature 60.0 - 120 °C
5080 - 7980 psi
@Temperature 140 - 248 °F
Average value: 43.3 MPa Grade Count:1
Tensile Strength, Yield 40.0 - 103 MPa5800 - 15000 psiAverage value: 57.2 MPa Grade Count:14
Elongation at Break 1.50 - 80.0 %1.50 - 80.0 %Average value: 7.89 % Grade Count:37
Elongation at Yield 3.00 - 7.00 %3.00 - 7.00 %Average value: 4.33 % Grade Count:3
Modulus of Elasticity 2.20 - 24.5 GPa319 - 3550 ksiAverage value: 5.67 GPa Grade Count:20
Flexural Yield Strength 55.0 - 186 MPa7980 - 27000 psiAverage value: 98.8 MPa Grade Count:30
Flexural Modulus 1.90 - 9.65 GPa276 - 1400 ksiAverage value: 4.79 GPa Grade Count:33
 2.50 - 5.00 GPa
@Temperature 60.0 - 120 °C
363 - 725 ksi
@Temperature 140 - 248 °F
Average value: 3.67 GPa Grade Count:1
Izod Impact, Notched 0.210 - 1.90 J/cm0.393 - 3.56 ft-lb/inAverage value: 0.579 J/cm Grade Count:20
 0.400 - 0.5339 J/cm
@Temperature -40.0 - -20.0 °C
0.749 - 1.000 ft-lb/in
@Temperature -40.0 - -4.00 °F
Average value: 0.445 J/cm Grade Count:2
Izod Impact, Unnotched 2.83 - 11.7 J/cm5.30 - 22.0 ft-lb/inAverage value: 5.27 J/cm Grade Count:4
Izod Impact, Notched (ISO) 3.00 - 15.0 kJ/m²1.43 - 7.14 ft-lb/in²Average value: 8.00 kJ/m² Grade Count:4
 <= 10.0 kJ/m²
@Temperature -30.0 - -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 10.0 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 25.0 - 25.0 kJ/m²
@Temperature -30.0 - -30.0 °C
11.9 - 11.9 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 25.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.50 J/cm² - NB7.14 ft-lb/in² - NBAverage value: 5.71 J/cm² Grade Count:9
 2.50 - 12.0 J/cm²
@Temperature -40.0 - -20.0 °C
11.9 - 57.1 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 5.13 J/cm² Grade Count:3
Charpy Impact, Notched 0.290 - 1.00 J/cm²1.38 - 4.76 ft-lb/in²Average value: 0.466 J/cm² Grade Count:17
 0.200 - 1.00 J/cm²
@Temperature -30.0 - -20.0 °C
0.952 - 4.76 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 0.507 J/cm² Grade Count:6
Tensile Creep Modulus, 1000 hours 1200 - 2000 MPa174000 - 290000 psiAverage value: 1500 MPa Grade Count:3
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+16 ohm-cm100 - 1.00e+16 ohm-cmAverage value: 5.14e+15 ohm-cm Grade Count:15
Surface Resistance 62.0 - 1.00e+15 ohm62.0 - 1.00e+15 ohmAverage value: 1.30e+14 ohm Grade Count:9
Dielectric Constant 3.50 - 4.003.50 - 4.00Average value: 3.70 Grade Count:8
Dielectric Strength 14.0 - 100 kV/mm356 - 2540 kV/inAverage value: 36.0 kV/mm Grade Count:10
Dissipation Factor 0.00120 - 0.03200.00120 - 0.0320Average value: 0.0132 Grade Count:4
Comparative Tracking Index 150 - 425 V150 - 425 VAverage value: 251 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 140 µm/m-°C3.89 - 78.0 µin/in-°FAverage value: 60.0 µm/m-°C Grade Count:13
 61.0 - 61.0 µm/m-°C
@Temperature 60.0 - 138 °C
33.9 - 33.9 µin/in-°F
@Temperature 140 - 280 °F
Average value: 61.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 50.0 - 110 µm/m-°C27.8 - 61.0 µin/in-°FAverage value: 83.3 µm/m-°C Grade Count:9
 88.0 - 88.0 µm/m-°C
@Temperature 60.0 - 138 °C
48.9 - 48.9 µin/in-°F
@Temperature 140 - 280 °F
Average value: 88.0 µm/m-°C Grade Count:1
Melting Point 210 - 255 °C410 - 491 °FAverage value: 227 °C Grade Count:17
Maximum Service Temperature, Air 100 - 345 °C212 - 653 °FAverage value: 245 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 110 - 215 °C230 - 419 °FAverage value: 176 °C Grade Count:28
Deflection Temperature at 1.8 MPa (264 psi) 48.9 - 206 °C120 - 402 °FAverage value: 106 °C Grade Count:32
Vicat Softening Point 170 - 205 °C338 - 401 °FAverage value: 186 °C Grade Count:5
Flammability, UL94 HB - V-0HB - V-0Grade Count:34
Glow Wire Test 650 - 960 °C1200 - 1760 °FAverage value: 753 °C Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 280 °C68.0 - 536 °FAverage value: 179 °C Grade Count:6
Nozzle Temperature 238 - 275 °C460 - 527 °FAverage value: 259 °C Grade Count:7
Melt Temperature 220 - 277 °C428 - 531 °FAverage value: 251 °C Grade Count:19
Mold Temperature 40.0 - 110 °C104 - 230 °FAverage value: 75.4 °C Grade Count:16
Drying Temperature 80.0 - 140 °C176 - 284 °FAverage value: 122 °C Grade Count:13
Moisture Content 0.000 - 0.200 %0.000 - 0.200 %Average value: 0.0540 % Grade Count:5
Vent Depth 0.00127 - 0.00380 cm0.000500 - 0.00150 inAverage value: 0.00253 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified

O3230 / 78181

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.