MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Riteflex® 655A TPC, Unfilled
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Riteflex 655A is a thermoplastic polyester elastomer with nominal shore D hardness of 55 and medium modulus.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Density of Compound 1.19 g/cc0.0430 lb/in³Indicative (PE only); ISO 1872-1
Water Absorption 0.40 %
@Temperature 22.8 °C
0.40 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inASTM D955
 0.016 - 0.019 cm/cm0.016 - 0.019 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.017 - 0.021 cm/cm0.017 - 0.021 in/inISO 294-4
Melt Flow 7.0 - 11 g/10 min7.0 - 11 g/10 minASTM D1238
 10 g/10 min
@Load 2.16 kg,
Temperature 220 °C
10 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
 555515 sec; ISO 868
Tensile Strength at Break 25.2 MPa3650 psiASTM D638
 30.0 MPa4350 psi50mm/min; ISO 527-2/1A
Tensile Strength, Yield 15.0 MPa2180 psi50mm/min; ISO 527-2/1A
Tensile Stress at Strain  8.00 MPa
@Strain 5.0 %
1160 psi
@Strain 5.0 %
ISO 527-1/2
 12.0 MPa
@Strain 10 %
1740 psi
@Strain 10 %
ISO 527-1/2
 15.0 MPa
@Strain 50 %
2180 psi
@Strain 50 %
ISO 727-1/2
 15.0 MPa
@Strain 50 %
2180 psi
@Strain 50 %
ISO 527-2/1A
Elongation at Break >= 300 %>= 300 %
 430 %430 %ASTM D638
Elongation at Yield 28 %28 %50mm/min; ISO 527-2/1A
Tensile Modulus 0.175 GPa25.4 ksi50mm/min; ISO 527-2/1A
 0.241 GPa34.9 ksiASTM D638
Flexural Strength 10.0 MPa1450 psiISO 178
 7.00 MPa
@Strain 3.5 %
1020 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 0.175 GPa25.4 ksiISO 178
 0.210 GPa30.5 ksiASTM D790
 0.0860 GPa
@Temperature 100 °C
12.5 ksi
@Temperature 212 °F
ISO 178
 0.677 GPa
@Temperature -40.0 °C
98.2 ksi
@Temperature -40.0 °F
ASTM D790
 0.700 GPa
@Temperature -40.0 °C
102 ksi
@Temperature -40.0 °F
ISO 178
Resilience 4848Bayshore, %; ASTM D2632
 4848Bayshore, %
Flex Crack Resistance >= 1.00e+6>= 1.00e+6Ross flex
Izod Impact, Notched NBNBASTM D256
 1.44 J/cm
@Temperature -40.0 °C
2.70 ft-lb/in
@Temperature -40.0 °F
ASTM D256
Izod Impact, Notched (ISO) NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 15.0 J/cm²71.4 ft-lb/in²partial break; ISO 179/1eA
 6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
partial break; ISO 179/1eA
Tear Strength 124 kN/m708 pliISO 34-1
 211.2 kN/m1205 pliASTM D624
 217 kN/m1240 pliASTM D1004
Compression Set <= 1.0 %<= 1.0 %ASTM D395
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.00e+12 ohm-cm4.00e+12 ohm-cmIEC 60093
 5.00e+12 ohm-cm5.00e+12 ohm-cmASTM D257
Surface Resistance 4.00e+15 ohm4.00e+15 ohmIEC 60093
Dielectric Constant 4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 13.8 kV/mm350 kV/inshort term; ASTM D149
 14.0 kV/mm356 kV/inIEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
 >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 200 µm/m-°C111 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 170 µm/m-°C94.4 µin/in-°FISO 11359-2
Melting Point 200 °C392 °F10°C/min; ISO 11357-1,-2,-3
 200 °C392 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 48.0 °C118 °FISO 75-1, -2
Vicat Softening Point 181 °C358 °FASTM D1525
Glass Transition Temp, Tg -56.7 °C-70.0 °FASTM D3418
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 55.0 °C68.0 - 131 °Fcavity
 205 - 235 °C401 - 455 °Fhot runner
Feed Temperature 200 - 215 °C392 - 419 °F
Zone 1 200 - 215 °C392 - 419 °F
Zone 2 205 - 230 °C401 - 446 °F
Zone 3 205 - 230 °C401 - 446 °F
Zone 4 205 - 235 °C401 - 455 °F
Die Temperature 205 - 235 °C401 - 455 °F
Melt Temperature 205 - 235 °C401 - 455 °F
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour
Moisture Content <= 0.050 %<= 0.050 %
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Processing typeInj/Blow/Ext

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Riteflex® 640A TPC, Unfilled
Celanese Riteflex® 435 TPC, Unfilled
Celanese Riteflex® 663 TPC, Unfilled
Celanese Riteflex® 655HS TPC, Unfilled
Celanese Riteflex® 672 TPC, Unfilled

PHCQ452 / 178907

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.